Mine aren't that way..are you using too much pressure? Which pads are they?
They are LC CSS pads. I also looked at the my Flex's Velcro backing plate, right in the middle where the bolt is there is a half-dollar size edge where the velcro melted.

I'm thinking a couple of explanations:

- the pad was defective, transferring heat to the backing plate and melting it

- the flex was defective, melting the plate and damaging the pad (unlikely b/c the white pad didn't have any problems)

- the pad got saturated w/ product, so i increased pressure for more cutting. this caused the pad to break down allowing heat to transfer to the back plate and melting the velcro.